SA07
Electrical
- Feb 22, 2018
- 373
Hi
We are replacing an existing Boiler feed pump of flow 21 m3/hr by 30 m3/hr. This is because we need more flow. The pump is in operation since 2015.
Flow 30m3/hr
Head 31 bar
Temperature 120deg C
Medium Boiler feed water pH 8.5-9.5 temp 120deg C
We have got several quotes. The quote of the OEM is 1.8x quote of other suppliers. Different suppliers have quoted different materials.
We are not designing a new boiler feed pump.
The OEM has quoted the following material:
Pump casing material CS WCB
Pump impeller material WCB MOC
Other supplier has quoted the following material:
Pump casing material EN-GJL-250
Pump impeller material Steel CrNi 1.4301
Can we use the materials (Pump casing material EN-GJL-250 Pump impeller material Steel CrNi 1.4301 ) for this boiler feed pump working at these conditions?
What material is recommended for the pump casing and pump impeller for a boiler feed pump at these operation conditions?
We are replacing an existing Boiler feed pump of flow 21 m3/hr by 30 m3/hr. This is because we need more flow. The pump is in operation since 2015.
Flow 30m3/hr
Head 31 bar
Temperature 120deg C
Medium Boiler feed water pH 8.5-9.5 temp 120deg C
We have got several quotes. The quote of the OEM is 1.8x quote of other suppliers. Different suppliers have quoted different materials.
We are not designing a new boiler feed pump.
The OEM has quoted the following material:
Pump casing material CS WCB
Pump impeller material WCB MOC
Other supplier has quoted the following material:
Pump casing material EN-GJL-250
Pump impeller material Steel CrNi 1.4301
Can we use the materials (Pump casing material EN-GJL-250 Pump impeller material Steel CrNi 1.4301 ) for this boiler feed pump working at these conditions?
What material is recommended for the pump casing and pump impeller for a boiler feed pump at these operation conditions?