From the Guardian UK, "The US government will order emergency checks of dozens of Boeing 737s after Southwest airlines was forced to ground planes over safety concerns.
Southwest cancelled hundreds of flights after a five-foot tear opened in the fuselage of a plane 20 minutes after taking off from Phoenix on Friday.
The Federal Aviation Administration has now ordered fuselage inspections of older 737-300, -400, and -500 models, involving what could be time-consuming and repetitive electromagnetic checks.
"This action is designed to detect cracking in a specific part of the aircraft that cannot be spotted with visual inspection," FAA administrator Randy Babbitt said.
Boeing will offer its own advice to airlines outlining specific inspection steps."
Dik
Southwest cancelled hundreds of flights after a five-foot tear opened in the fuselage of a plane 20 minutes after taking off from Phoenix on Friday.
The Federal Aviation Administration has now ordered fuselage inspections of older 737-300, -400, and -500 models, involving what could be time-consuming and repetitive electromagnetic checks.
"This action is designed to detect cracking in a specific part of the aircraft that cannot be spotted with visual inspection," FAA administrator Randy Babbitt said.
Boeing will offer its own advice to airlines outlining specific inspection steps."
Dik