What is the difference between stellite facing and integral seats for check valves?
 
Replies continue below

Recommended for you

Stellite is a hard facing material plated onto an integral seat. An integral seat is a seat that is formed into the metal body of the valve so the seat is part of the metal block of the valve.
 