We're going to repair B 737 floor panels. The SRM gives BMS 5- 107 (53-00-50) as the adhesive to use for the inserts. I can't find any reference anywhere for adhesives that meet this standard. It ought to be in 51-30-03 but it isn't.
Help!

Dan320
 
Supplier specs. for BMS 5-107:

Araldite 420 A/B
or
Epibond 420 A/B
 
Hi,

You can get a QPL (qualified suppliers list) for BMS 5-107 from myboeingfleet website. Normally, airlines / MRO who operates/maintains Boeing aircraft has access to this site.

The QPL contain the list of materials (in this case adhesive) meeting the specification with the corresponding supplier information.



Albert
 
Thank you guys. Really appreciate it.