Is using bluestone mixed with soil able to support a roadway?
 
Replies continue below

Recommended for you

technician06...your question doesn't offer enough background for adequate input.

First, "bluestone" is a colloquial term to describe certain greywhacke or sandstones. I assume you are somewhere in PA/WV/NY or somewhere along the middle ot upper Appalachians.

The material itself, if crusher run and well graded can serve as a base material or as a stabilization material when mixed with sand. Are you considering using spoil materials from a stone quarry operation where architectural stone is produced?

Can it support a roadway? That depends on the type of roadway and whether there are other components of the pavement section to consider. To mix bluestone alone with sand would not produce a very good "roadway", but would provide a good starting point for the building of a pavement section. Above that you would typically install a base material and above that, an asphaltic concrete layer or layers, depending on the traffic type, frequency, and other design conditions.
 