Please assist to correct information, In our BOP system, vendor are install brass fitting in ss line.
This dissimilar material are acceptable as per the engineering standard.
Attached snaps for your better information.

IMG-20210323-WA0001_bkyvrn.jpg
IMG-20210323-WA0002_raenj3.jpg
 
If this is stainless 301 or 304 and Brass the risk is low.

Where is your electrolyte (water etc) to form the corrosion cell? No water or electrolyte no corrosion