Oct 24, 2017 #1 kris hari Mechanical Joined Oct 24, 2017 Messages 2 Location KW what is light blasting?
Oct 24, 2017 #2 nackra Civil/Environmental Joined Oct 2, 2001 Messages 160 Location US basic descriptions can be found here: http://www.hydroflotech.com/steel-structures-painting-council-sspc-publications Upvote 0 Downvote
basic descriptions can be found here: http://www.hydroflotech.com/steel-structures-painting-council-sspc-publications
Oct 24, 2017 Thread starter #3 kris hari Mechanical Joined Oct 24, 2017 Messages 2 Location KW Thank you for the link. But my question is with regard to Internal lining of pipe . As per our client spec,the damaged area of internal lining of the pipe need to be light blasted and lining.This is not found in link(Light blast). Upvote 0 Downvote
Thank you for the link. But my question is with regard to Internal lining of pipe . As per our client spec,the damaged area of internal lining of the pipe need to be light blasted and lining.This is not found in link(Light blast).
Oct 24, 2017 #4 EdStainless Materials Joined May 20, 2004 Messages 16,363 Location Waukesha WI USA light blasting simply means that you do not have to blast back to a specific profile, just blast to assure that it is clean. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
light blasting simply means that you do not have to blast back to a specific profile, just blast to assure that it is clean. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Oct 24, 2017 2 #5 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Read about it,,,,,,,,,,,,,,, http://blastjournal.com/surface-preparation-standards-explained/ Upvote 0 Downvote
Oct 25, 2017 #6 21121956 Mechanical Joined Jul 29, 2005 Messages 420 Location HN Hello everybody: metengr, thanks for the link. Star for you. El que no puede andar, se sienta. Upvote 0 Downvote
Oct 26, 2017 #7 CoCoE Petroleum Joined Mar 9, 2012 Messages 118 Location JP Light blasting = brush off blast cleaning (SSPC SP-7) Upvote 0 Downvote