what is light blasting?
 
Thank you for the link. But my question is with regard to Internal lining of pipe . As per our client spec,the damaged area of internal lining of the pipe need to be light blasted and lining.This is not found in link(Light blast).
 
light blasting simply means that you do not have to blast back to a specific profile, just blast to assure that it is clean.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Hello everybody:

metengr, thanks for the link. Star for you.

El que no puede andar, se sienta.
 
Light blasting = brush off blast cleaning (SSPC SP-7)
 