For concrete, what is the purpose of the process of pelletization of granulation of blast furnace slag?
 
Pelletized Blast Furnace Slag

If the molten slag is cooled and solidified with water and air quenched in a spinning drum, pellets, rather than a solid mass, can be produced. By controlling the process, the pellets can be made more crystalline, which is beneficial for aggregate use, or more vitrified (glassy), which is more desirable in cementitious applications. More rapid quenching results in greater vitrification and less crystallization.

Granulated Blast Furnace Slag

If the molten slag is cooled and solidified by rapid water quenching to a glassy state, little or no crystallization occurs. This process results in the formation of sand size (or frit-like) fragments, usually with some friable clinkerlike material. The physical structure and gradation of granulated slag depend on the chemical composition of the slag, its temperature at the time of water quenching, and the method of production. When crushed or milled to very fine cement-sized particles, ground granulated blast furnace slag has cementitious properties, which make a suitable partial replacement for or additive to Portland cement.
 