We have several parts that are Carburized then blasted to remove machining burrs, had a part that is Ferritic Nitrocarb that has the potential of having some light burrs. The requirement is to have a .010mm white layer on the part, thoughts on blast deburring parts with this process and not damaging the working surface white layer?? I don't have much experience with FNC, but I know we won't want any damage to the white layer.
Thanks
 
EdStainless
Material is quite soft, but If need be deburring 1st is an option to develop.