Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Black Polyurethane Rubber Alternative 2

Status
Not open for further replies.

Alpacahontas

Mechanical
Aug 3, 2018
3
I'm tasked with finding a vibration damping rubber mount that is compatible with solvents and acetone. What other materials should I look for beside black polyeurethane rubber? Will simple urethane mounts work just as fine?

Thank you.
 
Replies continue below

Recommended for you

EPDM, Butyl (and halobutyl) compounds will work well with acetone and other ketones. As for the term "solvents", this is far too general to give you a more specific answer.

forumtowers.com
 
Thank you, I will look into those materials.

I'm not sure exactly which solvents but generally the stuff that is mixed in with photoresist in photolithography. The mounts are used in wafer coating machines before all solvents are baked out of the resists, hence the constant acetone and solvents exposure.
Sorry I can't be more specifics due to troubles contacting our engineers.
 
The colour of the rubber has little influence on the chemical resistance. I would advice against (black) (poly)urethane rubber if you use aceton (+ other solvents).
 
Status