Quality2479
Materials
Hi,
What ideal joint preparation would be for a shell horizontal seam joint in Tanks of thickness 15mm and above-
1. Single Bevel Preparation in one shell course (Top) and other shell course without any kind of bevel preparation by keeping edges square.
or
2. Double Bevel Preparation in one shell course (Top) and other shell course without any kind of bevel preparation by keeping edges square.
Is there any standard or any kind of literature mentioning the requirements of bevel preparation or bevel preparation which changes as per the thickness & position of welding.
Thanks
What ideal joint preparation would be for a shell horizontal seam joint in Tanks of thickness 15mm and above-
1. Single Bevel Preparation in one shell course (Top) and other shell course without any kind of bevel preparation by keeping edges square.
or
2. Double Bevel Preparation in one shell course (Top) and other shell course without any kind of bevel preparation by keeping edges square.
Is there any standard or any kind of literature mentioning the requirements of bevel preparation or bevel preparation which changes as per the thickness & position of welding.
Thanks