Our procedure for welding 304 SS (ASTM A204) to HSLAS-F (A1008 Grade 50) calls for ER309L (GTAW). Materials less than 1/2-inch thk. Preheat is 350F, no post weld HT. We have found the HSLAS-F to have slightly higher carbon than spec allows, .3% vs .15%. Is the ER309L filler still best choice?
Thanks.