Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Best Oring material for 20 year seawater seals

Status
Not open for further replies.

jimoosse

Marine/Ocean
Joined
Jan 31, 2013
Messages
1
Location
US
I know Nitrile (NBR) is usually recommended for normal seawater sealing applications. I have a job that will be unserviced for 20 years, at ~2000 psi, 2 degrees C.

Nitrile or EPDM? A few sources tout EPDM as better for seawater but most dont.

and 70 duro or 90 duro?

They are all titanium housings with both face and piston seals.

Any reports or links would be really helpful.

thanks everyone.
 
20 years is a big ask! Are the piston seals dynamic seals? Have you considered polymer seals to achieve 20years?

Send a sketch so we can see where the seals are located.
 
You have to consult with the manufacturers. Slight differences in rubber formulation or quality will have major effects on life-span.
 
Status