What are your thoughts on the best lubricant or protector I could use to prevent saltwater corrosion. I am looking for something to treat my outboard motor, along with hardware on my boat to help prevent corrosion. I currently use "T-9" but was wondering if there is any kind of grease or lubricant out there that might be better?

thanks for any ideas!
 
Replies continue below

Recommended for you

Are your refering to internal or external corrosion? For a good external top coat protection we use Nyalic polymer resin coating (clear).
 
Thanks for the reply.

Sorry I should have specified. Yes External. Is this Nyalic polymer resin coating easy to find?
 
We ordered it from Palm Industries 1-800-643-7851
 
WHEN DID YOU PURCHASE NYALIC FROM PALM INDUSTRIES?
 
We have purcased it several times over the last 2 years. In the marine enviroment it performs great. Good luck

 