Conveyor support diagonal members got bent from careless lifting. Anyone know enough to recommend should we replace the members or can we use as-is?

7F04F4A1-E35E-4466-B93E-1A7BF93A577F_bwzlj4.jpg

7E8A4FAB-7340-4890-BF7D-DAC093EE6D56_axhkpq.jpg
2CDCE58D-9964-4A3F-A1A7-F8E73171551B_ljdjnm.jpg
86A62146-19F9-4FB7-BD41-C9418136CC6A_efpuae.jpg
8BC54795-3B0D-44FF-8402-C6006B80F79E_jxnrhq.jpg
DFE14288-1447-431A-B42A-6A1EBBDBD5E2_vhnupd.jpg
 
Replies continue below

Recommended for you

In some cases, diagonal bracing can be designed as tension-only members, and local flange dings likely wouldn't reduce the tensile strength.
I would think some of those spots could be repaired by cutting out small areas of the angle rather than replacing the whole angle. Or possibly using heat and applied force to straighten what's there.
 
My $.02:

1) Based on the pictures, those diagonals are both tension and compression

2) What's your relationship to the situation? Are you the owner, owner's engineer, engineer for the conveyor company, or engineer for the company that provided the supports?

3) The owner is buying a new system, which includes the support. If you were buying something new, would you accept it in a "not-pristine" condition? What kind of additional warranty would you want before taking possession? As SRE mentioned, some of the welds may have been damaged. Who's going to own the welds in their current state?

Especially because it's brand new, I would have the damaged members replaced, at a minimum. Due to the HDG, I could probably make a strong argument for having a new support constructed (depending on the actual corrosion mitigation needs coupled with the labor for welding HDG), though time-constraints may over-rule that idea.
 
We are the owners and it was our employees who where negligent unfortunately. They are used pieces that are being repurposed.

It sounds like we should replace the members.

Thanks guys
 
Options that come to my mind:

1. Replace.

2. Do an analysis that takes into account the new eccentricities & damage.

3. Bolt some new angles to the old ones. (I.e. reinforcement.)
 
USAeng:
Well..., at least you know who to blame, and who to sue when things start going south. I would think that most of that damage can be fixed with a little engineering imagination, judgement and experience. It will take a little structural analysis and understanding of how the various members function in the structure, and under what loads, etc., but since it is being repurposed, in house, most of that should already have been done. Some gentle straightening with a hammer, a come-along or a hydraulic jack, maybe a little heat would certainly be in order. Examine the member, welds and joints for ripping which could grow or reduce cap’y. If they are tension members you don’t want to have reduced the net area or allowed a nick/ripped area which can rupture under a tensile loading. If they are compression members the primary concern is slenderness, stiffness and the potential of column type buckling. In both cases a reinforcing angle added over the existing angle would normally be enough. Grind the corners so you get good fit-up and weld the two together. If the material is HDG you would have some welding problems, and the people doing the work should know what they are doing and do quality work, not just be able to melt welding rods. You might want to talk with your local fabricator who could supply the material, and send the right equipment and a qualified crew out for a day or so.
 