I have a consultation regarding the bending test of titanium alloy welding
ISO 15614-5
Quote
The diameter of the former or the inner roller shall be 6 t except for material group 51 when 4 t shall be used. The bending angle shall be 180° for parent metal with elongation A ≥ 20%. For parent metal with elongation A < 20% the following formula shall apply:
d=(100*ts)/10-ts
Unquote
(1) Bending angle and bending diameter for group 51 with elongation A < 20%
Which of the following viewpoints is correct?
a) Bending angle shall be 180° and bending diameter shall be calculated according to the formula
b) Bending angle shall be 180° and bending diameter shall be 4t
(2) Bending angle and bending diameter for material group other than group 51. The elongation of all material groups :A < 20%
Which of the following viewpoints is correct?
a) Bending angle shall be 180° and bending diameter shall be calculated according to the formula
b) Bending angle shall be 180° and bending diameter shall be 6t
ISO 15614-5
Quote
The diameter of the former or the inner roller shall be 6 t except for material group 51 when 4 t shall be used. The bending angle shall be 180° for parent metal with elongation A ≥ 20%. For parent metal with elongation A < 20% the following formula shall apply:
d=(100*ts)/10-ts
Unquote
(1) Bending angle and bending diameter for group 51 with elongation A < 20%
Which of the following viewpoints is correct?
a) Bending angle shall be 180° and bending diameter shall be calculated according to the formula
b) Bending angle shall be 180° and bending diameter shall be 4t
(2) Bending angle and bending diameter for material group other than group 51. The elongation of all material groups :A < 20%
Which of the following viewpoints is correct?
a) Bending angle shall be 180° and bending diameter shall be calculated according to the formula
b) Bending angle shall be 180° and bending diameter shall be 6t