I am planning to make a cage from 1/8" stainless steel flat plate. The plate will be cut with a water jet. After it is cut, I will need to bend the cage to conform to the front of a helmet. The overall dimension of the cage will be roughly 6" wide by 12" long.
What is the best way to bend this material? I've looked at roller machines, but they all seem to cap out at about 20ga. for the smaller machines. Should I look at a hydraulic press and a form to bend the cage into?
Thanks in advance for your help!
I am planning to make a cage from 1/8" stainless steel flat plate. The plate will be cut with a water jet. After it is cut, I will need to bend the cage to conform to the front of a helmet. The overall dimension of the cage will be roughly 6" wide by 12" long.
What is the best way to bend this material? I've looked at roller machines, but they all seem to cap out at about 20ga. for the smaller machines. Should I look at a hydraulic press and a form to bend the cage into?
Thanks in advance for your help!