We are preparing a PQR for welding Aluminum bronze and I am unsure if this material is too brittle to get face and root bends.

We have materials for one "testing" and I am outside of USA and can't replace soon. Did anyone else have any luck with this and is there some justification to do side bends instead?
 
From my experience with boat propellers, aluminum bronze is certainly not too brittle to be bent.
 
I've never hada problem bend testing wrought AL-bronze ASME IX weld procedure qualifictions. I've never had to test cast Al-bronze for PQR testing.
 