Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Bearing roughness specification

clon

Automotive
Joined
Apr 25, 2025
Messages
2
I am designing a customized TRB (Tapered Roller Bearing) and I need to define the roughness of inner and outer rings raceways and the roughness of the rollers. I would like to do it with respect to Ra and Rsk. The latter (Rsk) is particularly important because when it has negative values, the valleys of the roughness profile behave as little "tanks" for the lubricating oil, ensuring a proper lubrication.

Does someone know which Rsk values are typical used for bearings raceways? I cannot find anything in literature
 
Tapered roller bearings are not hydrodynamic bearings. They do not require reservoirs of oil. High and low spots increase contact pressure and shorten the life of the bearing. Smoother is better.
 
Many studies in the literature (e.g., https://www.mdpi.com/2075-4442/8/7/76) confirm that even for TRBs negative skewness can be beneficial. The idea is to have a smooth surface and these pits as reservoirs for oil and to reduce contact pressure. The issue is that I couldn't find any stated values of Rsk.
 
One thing to keep in mind is that Rsk is VERY unstable when trying to measure it on real surfaces. A single pit or pore can drastically change the result. A better approach might be to look at average valley depth (Rv ISO, Rvm ASME) as compared to average peak height (Rp ISO, Rpm ASME). Alternatively, there are many other parameters than can be considered.
 
Tapered roller bearing raceways are ground to achieve a very smooth surface, typically with a surface roughness Ra (average roughness) value of less than 0.4 μm (micro-meters) according to some bearing manufacturers.

The rolling elements are typically in the same range. What you DON'T want is something too smooth - the element then tends to "skid" instead of roll.
 