Nov 20, 2003 #1 rdmrr Marine/Ocean Joined May 30, 2003 Messages 3 Location US Hi, On a steel drawing done in 1958, steel piles are shown to be 10"x10" B.P. 42# beam. Can somebody help me to get the main dimensions of the beam? Regards, rdmrr
Hi, On a steel drawing done in 1958, steel piles are shown to be 10"x10" B.P. 42# beam. Can somebody help me to get the main dimensions of the beam? Regards, rdmrr
Nov 20, 2003 1 #2 Iskit4iam Mechanical Joined Jun 20, 2001 Messages 63 Location US From the 1956 AISI Steel Construction Manual 10 x 10 BP 42 is an H piling Depth paralell to the web 9.72 Width 10.078 Flange thickness .418 Web thickness .418 42 Lbs per foot Area 12.35 Ixx 210.8 Sxx 43.4 rxx 4.13 I'yy 71.4 S'yy 14.2 r'yy 2.4 Upvote 0 Downvote
From the 1956 AISI Steel Construction Manual 10 x 10 BP 42 is an H piling Depth paralell to the web 9.72 Width 10.078 Flange thickness .418 Web thickness .418 42 Lbs per foot Area 12.35 Ixx 210.8 Sxx 43.4 rxx 4.13 I'yy 71.4 S'yy 14.2 r'yy 2.4
Nov 21, 2003 Thread starter #3 rdmrr Marine/Ocean Joined May 30, 2003 Messages 3 Location US Thanks Iskit4iam. It is very helpful. Regards, rdmrr Upvote 0 Downvote