On a steel drawing done in 1958, steel piles are shown to be 10"x10" B.P. 42# beam.

Can somebody help me to get the main dimensions of the beam?

Regards,

rdmrr
 
From the 1956 AISI Steel Construction Manual

10 x 10 BP 42 is an H piling

Depth paralell to the web 9.72
Width 10.078
Flange thickness .418
Web thickness .418
42 Lbs per foot

Area 12.35

Ixx 210.8
Sxx 43.4
rxx 4.13

I'yy 71.4
S'yy 14.2
r'yy 2.4
 
Thanks Iskit4iam.

It is very helpful.

Regards,

rdmrr
 