Hello all
I am currently using Be-cu alloy for a connector. I am planning to change this material to an alternative.
Be-Cu - C17300 UNS
This connector is used in coaxial cable where a male pin is inserted between the crimped fingers in a female pin. The crimped fingers should last the insertion/widhrawal force cycle. The insertion/widhrawal force is approx. 0.80lbs
Thanks