Could anyone tell me what they use for Bituminous Coated Corrugated Metal Pipe (BCCMP) manning's n value? Please include your reference if you have one handy. Thank you much.
 
Replies continue below

Recommended for you

same as regular CMP - generally accepted as 0.024
 
cvg or dicksewerrat.... do you happen to have any widely used reference manual for this information? My bently stormwater manual does not show BCCMP. I appreciate the responses.
 
just use your reference for normal cmp. the coating does not have a significant effect on the roughness
 