Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ball valve material

Status
Not open for further replies.

surtigaf

Materials
Joined
Feb 10, 2003
Messages
2
Location
BR
Can anyone tell me what is the difference between AISI 410 & ASTM A217 CA15. I tried to purchase a ball valve with a AISI 410 ball, but they only offer a valve with a ASTM A217 CA15 ball and said it will be same material. Is this true. My I have any problem using one instead of another?
Sincerely,
Surtigaf
 
ASTM A 217 is a standard for martensitic stainless steel castings. Type 410 is a wrought stainless steel designation.
 
We can offer you Ball valves with both types of Balls i.e. with 410 or CA15 material. Basically it depends on the working pressure and temperature of the valve or line.

You can contact our company Leader valves Limited at the wb address leadervalves.com
 