Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ball & Socket O-ring (split o-ring)

Status
Not open for further replies.

mecoman

Mechanical
Dec 11, 2006
36
Hello,

Looking for a source for a split ball and socket o-ring. 1/8" diameter nom. dimension for a 5-1/8" shaft diameter. Needs to be fda approved EPDM and or FKM. It does NOT need to be white.


Thanks for your help,

MECOMAN

 
Replies continue below

Recommended for you

The only company that I have heard of that made such an o-ring was Chesterton. It was used in their split seal design in the late 1990's. I don't know if they still use this design or not. You should contact someone with Chesterton to see.

Johnny Pellin
 
Hello gentlemen...

I can confirm that Chesterton still uses the "ball and socket o'ring" on all split mechanical seals, but for some reason it is NOT available for individual purchase.

I believe you will find that this o'ring will be rather difficult to find, as Chesterton still owns the patent.

 
Greetings, there is a company in Florida that sells by the ea. the split o rings, the size you are looking for is listed as a (dash) - 42 o-ring. you can contact them at 863-425-9611 to help
 