We have a pump (high temp service 350 deg C)- sp gr 0.8; flow: 160m3/hr' diff head: 35 mts; etc.
This pump had a history of bearing failures. A decision was taken (after due consultations with OEM, i guess) to drill balancing holes in the impeller to reduce loads on the bearing.
After installation, the pump was reported to be not delivering the required head (ie "poor performance" according to operators).
Can anyone tell me what could be happening here.
We recently took this pump to workshop and inspected the internals: Wearing ring clearances are about 0.5 ~ 0.6 mm; impeller diameter appx 205 mm. Casing and impeller good condition (internally). Bearing condition was good.
Regards
This pump had a history of bearing failures. A decision was taken (after due consultations with OEM, i guess) to drill balancing holes in the impeller to reduce loads on the bearing.
After installation, the pump was reported to be not delivering the required head (ie "poor performance" according to operators).
Can anyone tell me what could be happening here.
We recently took this pump to workshop and inspected the internals: Wearing ring clearances are about 0.5 ~ 0.6 mm; impeller diameter appx 205 mm. Casing and impeller good condition (internally). Bearing condition was good.