i am looking for some information on baking porex. Currently the porex comes in rough and wavy...after baking at 279 f for 14 hours the porex becomes flat. Please note our only objective is for hard and flat porex. I doubt whether we require a 14 hour cycle time . Looking for help from those who are involved in a similar process.

-mechantaeus
 
Replies continue below

Recommended for you

If you just need it hard an flat try vacplate instead of the porex. It is sold in sheets.
 
Can anyone give me more info on VACPLATE. Does it need to be baked like porex? Is it better than porex etc.

Thanks,
-mechantaeus
 
Try Porvair Filtration Group, they also make porous plastic like Porex, trade name is Vyon. It is regularly used in vacuum pads.

(US Sales Office)
454 South Anderson Road,
BTC 514, Rock Hill, SC 29730
USA
T: +1 803 327 5008
F: +1 803 327 1052

or
Wrexham, UK
T: +44 1978 661144
F: +44 1978 664554

See
 
Status
Not open for further replies.

Similar threads

Part and Inventory Search

Sponsor