Yes, eletrogalvanized bake hardening steels can be welded. The appropriate standards are SAE J1562 Selection of Zinc and Zinc-Alloy (Hot-Dipped and Electrodeposited Coated Steel Sheet and SAE J2340 Categorization and Properties of Dent Resistant, High Strength, and Ultra High Strength Automotive Sheet Steel.