Metalsmythe1977, all... very odd response from Your vendor...
NASM1312-8 FASTENER TEST METHODS, METHOD 8, TENSILE STRENGTH
1. SCOPE
1.1 Applicability. This method covers a procedure for testing all types of structural fasteners in axial tension at room
temperature. This procedure is intended to define the test required to determine the tensile strength of the fastener
itself, not the strength of the fastener in any combination of sheet materials, sheet heat treat levels, or sheet
thicknesses.
FIGURE 1 – TENSION FIXTURES FOR SHORT GRIP FASTENERS
There are tension-test fixtures for short-grip fasteners.