Jul 13, 2006 #1 beidlerj Mechanical Joined Jul 13, 2006 Messages 2 Location US i am searching for basic allowable stresses for the following material which is not listed in B31.3: SB-705 N06625 60Ni - 22Cr - 9Mo - 3.5Cb Wld. Pipe Annealed in the -20 to 1000 degF range many thanks.
i am searching for basic allowable stresses for the following material which is not listed in B31.3: SB-705 N06625 60Ni - 22Cr - 9Mo - 3.5Cb Wld. Pipe Annealed in the -20 to 1000 degF range many thanks.
Jul 17, 2006 1 #2 ytse Mechanical Joined Aug 6, 2002 Messages 41 Location CA B-705 N06625 is listed in Table A-1 of ASME B31.3. SB is ASME spec (same material) listed under the Boiler Pressure Vessel Code. For B31.3 piping you can use the allowable stresses of the B-705 material in B31.3. Upvote 0 Downvote
B-705 N06625 is listed in Table A-1 of ASME B31.3. SB is ASME spec (same material) listed under the Boiler Pressure Vessel Code. For B31.3 piping you can use the allowable stresses of the B-705 material in B31.3.