I am looking for the correct value of allowable stress
to be assumed for ASTM B705.

Many thanks in advance
 
Replies continue below

Recommended for you

Which material are you interested in and what design temperature?

SB-705 N06625 60Ni - 22Cr - 9Mo - 3.5Cb Wld. Pipe Annealed

SB-705 N08825 42Ni - 21.5Cr - 3Mo - 2.3Cu Wld. Pipe Annealed


 