Is there anything in B31.3 indicating a two pass cap on a socket weld, or is this more of an engineering recommendation?
 
Replies continue below

Recommended for you

Your suspicions are correct. Code is silent, so the prudent "2 pass minimum" belongs in your company wilding specification.

And yes, I always require a 2-pass minimum. Have seen a number of single-pass welds leak, over the years.
 