Good day all,
I currently have a piping specification which calls out for material of SA-358 304H Cl.1 at 850 degF. In trying to calculate the minimum thickness using B31.3, I am not finding this material in the allowable stresses section.
Checking ASME Sec. 2D, I find the material however it only gives me stress values up to 800 degF.
Is there a different section that I am missing or looking at the wrong material in the ASME codes ?
I currently have a piping specification which calls out for material of SA-358 304H Cl.1 at 850 degF. In trying to calculate the minimum thickness using B31.3, I am not finding this material in the allowable stresses section.
Checking ASME Sec. 2D, I find the material however it only gives me stress values up to 800 degF.
Is there a different section that I am missing or looking at the wrong material in the ASME codes ?