Hi Every one
We have been discussing about para 323.3.4 ASME B31.3 2008, we all understand that it is required to reduce the test temperature for sub-size impact test specimens as per table Table 323.3.4. But none of us could explain why.
Please share your thought.
Thanks
MIKE
We have been discussing about para 323.3.4 ASME B31.3 2008, we all understand that it is required to reduce the test temperature for sub-size impact test specimens as per table Table 323.3.4. But none of us could explain why.
Please share your thought.
Thanks
MIKE