Hi,
Can someone help me with a question regarding B16 studs? I have a B16 stud on a floating head that is experiencing H2/H2S (Cooper-Gourman) corrosion. I am trying to avoid specifying B8 class 2 (strain hardened stainless steel) because of a chloride SCC concern. I remember that there is a stud made of a nickel base alloy but I cannot remember the ASTM number. Can someone help me?
Can someone help me with a question regarding B16 studs? I have a B16 stud on a floating head that is experiencing H2/H2S (Cooper-Gourman) corrosion. I am trying to avoid specifying B8 class 2 (strain hardened stainless steel) because of a chloride SCC concern. I remember that there is a stud made of a nickel base alloy but I cannot remember the ASTM number. Can someone help me?