Sep 6, 2002 #1 PAN Mechanical Joined Apr 25, 2001 Messages 549 Location SG For alloy 400, the user's requiremnet is flat bar (12 mm. thickness, 90 mm. width). What's the suitable reference ASTM B127 or B164?
For alloy 400, the user's requiremnet is flat bar (12 mm. thickness, 90 mm. width). What's the suitable reference ASTM B127 or B164?
Sep 6, 2002 1 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US ASTM B 164 defines a bar as being at least 3.2 mm thick and up to 254 mm wide, so you should order this material according to ASTM B 164. Upvote 0 Downvote
ASTM B 164 defines a bar as being at least 3.2 mm thick and up to 254 mm wide, so you should order this material according to ASTM B 164.