Hi,

I'm design membrane bioreactor in wastewater plants and want to calculate the head lost of the membranes...
Does anyone know what can i take to calculate the flat sheet membrane's head lost?or where can i learn?

Thanks for any advice
 
Replies continue below

Recommended for you

Dear sir

Which type of flat membrane - ORELIS (France) from Novasep group produce flat sheet membrane which are used, since many years, inside MBR unit worldwide
Visit web site and feel free to ask question
Best regards
 
Typically, flat sheet MBR's have a transmembrane pressure (head loss across membranes) of about 1-3 psi. This is true of Kubota's flat sheet product and others are pretty much the same.
 