tiagoandrei
Electrical
Hello guys,
We are facing an interesting problem in a synchronous generator (4 Poles , 1800 RPM , nominal power 6.5 MW) driven by a gas turbine and gearbox. The shaft is presenting an axial movement (~1,5 Hz) when the load is about 1.6 MW.
Apparentely, the load (active or reactive) in the generator doesn't have any relation with frequency of the movement or its amplitude. We have conducted a lot of tests to comprove this theory.
The axial bearing was damaged by a continous operation of this turbogenerator on this condition. Actually is an single sleeve radial-axial bearing.
We have checked for misalignment between generator and gearbox. A little deviation from manufactur recommendations were verified. Although alignment were corrected, the problem still persist.
We also have conducted a lot of inspections in coupling (gear coupling) looking for something wrong but nothing were observed.
I have read some threads in this forum about the "hunting magnetic center" phenomenon present in eletric motor, but nothing regarding generators. It can also happen ?
We are facing an interesting problem in a synchronous generator (4 Poles , 1800 RPM , nominal power 6.5 MW) driven by a gas turbine and gearbox. The shaft is presenting an axial movement (~1,5 Hz) when the load is about 1.6 MW.
Apparentely, the load (active or reactive) in the generator doesn't have any relation with frequency of the movement or its amplitude. We have conducted a lot of tests to comprove this theory.
The axial bearing was damaged by a continous operation of this turbogenerator on this condition. Actually is an single sleeve radial-axial bearing.
We have checked for misalignment between generator and gearbox. A little deviation from manufactur recommendations were verified. Although alignment were corrected, the problem still persist.
We also have conducted a lot of inspections in coupling (gear coupling) looking for something wrong but nothing were observed.
I have read some threads in this forum about the "hunting magnetic center" phenomenon present in eletric motor, but nothing regarding generators. It can also happen ?