Is there a repair code similar to API 653 but for AWWA D-100 tanks?
 
Replies continue below

Recommended for you

Nope.

About 30 years ago, D-100 and API-650 were identical. This tells me that using API-653 for repairs and estimation Remaining Life is appropriate.
 
There used to be an AWWA standard for tank repair, but it has been withdrawn for years, I think.

You could use API-653 to the extent desired. However, base-design AWWA tanks don't include provisions for brittle fracture. And leak-prevention is desirable, but not as critical as with an oil tank. So some of the API-653 provisions could be relaxed considerably.
 