What is the AWS spec for the titanium weld wire I should buy for welding Titanium Gr.7 material? (plate)

Thanks,
 
Replies continue below

Recommended for you

According to the Ti-Handbook from TIMET, Table 23, use AWS 5.16 ERTi-7
 