Nov 5, 2007 #1 cmn8226 Mechanical Joined Apr 2, 2007 Messages 32 Location US What is the AWS spec for the titanium weld wire I should buy for welding Titanium Gr.7 material? (plate) Thanks,
What is the AWS spec for the titanium weld wire I should buy for welding Titanium Gr.7 material? (plate) Thanks,
Nov 5, 2007 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US According to the Ti-Handbook from TIMET, Table 23, use AWS 5.16 ERTi-7 Upvote 0 Downvote
Nov 5, 2007 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,947 Location GB Which is the same as the recommendation in AWS G2.4. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdoweb/ Upvote 0 Downvote
Which is the same as the recommendation in AWS G2.4. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdoweb/