Oct 21, 2013 #1 BSC111 Structural Joined Sep 9, 2004 Messages 4 Location US Can anyone tell me if there are any prequalified joints or procedures for rebar welding?
Oct 22, 2013 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US Depending on the applicable Code year, yes, but to the best of my recollection, it is specific to fillet welding of rebar to plate only, not rebar to rebar connections.
Depending on the applicable Code year, yes, but to the best of my recollection, it is specific to fillet welding of rebar to plate only, not rebar to rebar connections.
Oct 22, 2013 #3 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US Check AWS D1.4 Structural Welding Code-Reinforcing Steel