Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AWS D1.1 welding Code

Status
Not open for further replies.

421051

Specifier/Regulator
Apr 15, 2004
1
The AWS D1.1 welding code is talking of the "Rule of Eight". Does anybody knows what it is all about?
Thanks.
 
Replies continue below

Recommended for you

Code Clinic For Study of AWS D1.l Structural Welding Code – Steel R E F E R E N C E M A N U A L
Code Rules, in 8 sections, are as follows:
1. General Requirements
2. Design of Welded Connections
3. Prequalification of WPSs
4. Qualification
5. Fabrication
6. Inspection
7. Studwelding
8. Strengthening and Repairing Existing StructuresAlso,

AWS DI .l/D1 .I M:2002 18th Edition abstract states:
This code covers the welding requirements for any type of welded structure made from the commonly used carbon and low alloy constructional steels. Sections 1 through 8 constitute a body of rules for the regulation of welding in steel construction.
There are twelve mandatory and twelve non-mandatory annexes in this code. A Commentary of the code is included with
the document.