AWS D1.1, Table 4.4 lists the testing requirements for Fillet Welds. Essentially the table indicates
only Macroetch test speciments are required for fillet welds. Footnote (b) states all test speciments shall be visually inspected per 4.9.1
Based on that, the only test required for Fillet Weld PQR is visual inspection of macroetched specimens. Does anyone agree / disagree with that?
The last line in Table 4.4 discusses Groove Test. Footnote (d) talks about the requirement for CJP Groove Weld test plate.
Question: Why is Groove Test listed under Table 4.4 which is for Fillet Welds? The wording in footnote (d) is not at all clear (at least in my non-welding expert mind).
only Macroetch test speciments are required for fillet welds. Footnote (b) states all test speciments shall be visually inspected per 4.9.1
Based on that, the only test required for Fillet Weld PQR is visual inspection of macroetched specimens. Does anyone agree / disagree with that?
The last line in Table 4.4 discusses Groove Test. Footnote (d) talks about the requirement for CJP Groove Weld test plate.
Question: Why is Groove Test listed under Table 4.4 which is for Fillet Welds? The wording in footnote (d) is not at all clear (at least in my non-welding expert mind).