Hello All,
It recently came to my attention that we make Tjoint in W sections using a full pen B-U4b-GF weld on the flanges and opposing 1/4" fillet welds on the webs and flanges one jointing beam is smaller (see the attached picture).
In my reading of the code and looking at our weld procedure I have come to the conclusion that this may not be acceptable. Fistly our structural welding procedure is prequalified for the B-U4b-GF joint only and makes no mention of fillet welds. Unlike BPVC section IX wich extend butt welds to fillets D1.1 does not apear to do so. Futher more I can't find a way to justify the use of this joint design per the code rules. It seems I need full pen welds on these joints.
My questions are as follows.
1) Can I Justify the use of this joint design, and how would I go about doing so. If not, where in the code does it say so (I will get indescribable pressure to prove the case when I bring this forward to managment)
2) If I can use this joint design, how do I develop an AWS complient weld procedure for this type of joint.
I will greatly appreciate any help on this matter.
A question properly stated is a problem half solved.
Always remember, free advice is worth exactly what you pay for it!
It recently came to my attention that we make Tjoint in W sections using a full pen B-U4b-GF weld on the flanges and opposing 1/4" fillet welds on the webs and flanges one jointing beam is smaller (see the attached picture).
In my reading of the code and looking at our weld procedure I have come to the conclusion that this may not be acceptable. Fistly our structural welding procedure is prequalified for the B-U4b-GF joint only and makes no mention of fillet welds. Unlike BPVC section IX wich extend butt welds to fillets D1.1 does not apear to do so. Futher more I can't find a way to justify the use of this joint design per the code rules. It seems I need full pen welds on these joints.
My questions are as follows.
1) Can I Justify the use of this joint design, and how would I go about doing so. If not, where in the code does it say so (I will get indescribable pressure to prove the case when I bring this forward to managment)
2) If I can use this joint design, how do I develop an AWS complient weld procedure for this type of joint.
I will greatly appreciate any help on this matter.