bernoullies123
Mechanical
I am currently on a project where a large portion of the structural welds are under the 6GR position. AWS in their commentary clearly note that this type of weld needs to be done by specialized welders due to the difficultly of the weld joint configuration.
With that said, we are currently experiencing 5%+ repair rates per linear length and over 40% repair rate per joint calculation.
A root cause analysis etc. is being performed to determine the cause, with initially consensus is that the primary concern is in the parameters specified in the procedure.
Anyway I was just wanted to get any feedback from others on typical repair rates noted on their projects specific to 6GR welding.
Thanks in advance.
With that said, we are currently experiencing 5%+ repair rates per linear length and over 40% repair rate per joint calculation.
A root cause analysis etc. is being performed to determine the cause, with initially consensus is that the primary concern is in the parameters specified in the procedure.
Anyway I was just wanted to get any feedback from others on typical repair rates noted on their projects specific to 6GR welding.
Thanks in advance.