As per Table 4.2 (footnote d) of AWS D1.1-2010, a CJP also qualifies for PJP and fillet (see 4.11.3).
4.11.3 requires 3 macro test if we will also include PJP in the WPS (CJP & PJP) but if we only use CJP & Fillet in the WPS, do we still have to do macro test?
Thanks
As per Table 4.2 (footnote d) of AWS D1.1-2010, a CJP also qualifies for PJP and fillet (see 4.11.3).
4.11.3 requires 3 macro test if we will also include PJP in the WPS (CJP & PJP) but if we only use CJP & Fillet in the WPS, do we still have to do macro test?