Jan 18, 2005 #1 damc Aerospace Joined Jan 10, 2003 Messages 14 Location US Can anyone tell me if Phosphor Bronze UNS C52400 is available in round bars over 4 inch dia. and if so where?
Can anyone tell me if Phosphor Bronze UNS C52400 is available in round bars over 4 inch dia. and if so where?
Jan 18, 2005 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Here you go, check with these folks; http://www.nbm-houston.com/c510.html Upvote 0 Downvote