Here is a report that I ran across from ONRL. You might also want to check their website, Ceramic Technology for further information.
Peter J. Blau, Rebecca L. Martin, and Laura Riester, "A Comparison of Several Surface Finish Measurement Methods as Applied to Ground Ceramic and Metal Surfaces," Ceramic Technology Project Report ORNL/M-4924, January 1996.